Heat treatment of metals and alloys includes a range of technological processes aimed at changing the parameters, configuration and qualitative properties of alloys or metals. One of the most important methods is thermochemical treatment of metals, which makes it possible to significantly change the properties of the metal, in particular its surface layer.
Metal treatment methods
Metal processing is divided into several main types:
- Heat treatment.
- Thermochemical treatment.
- Electrophysical treatment.
- Electrochemical treatment.
- Other methods.
Heat treatment of metals
Heat treatment changes the structure of a material through heating, soaking and cooling. These operations lead to hardening, softening and stabilization of the metal. The main types of heat treatment include:
- Annealing: the workpiece is heated and then slowly cooled in the furnace, relieving residual stresses, increasing ductility and reducing the hardness of the metal.
- Hardening: steel is heated above the critical point and rapidly cooled, which increases strength and reduces the ductility of the metal.
- Tempering: hardened metal is heated to a certain temperature, held and then cooled, which reduces internal stresses and makes the workpiece more ductile.
- Normalizing: the workpiece is heated and cooled in air. It is a more economical and faster alternative to annealing.
- Aging: the material is made to change, quickly, properties that would otherwise change very slowly under normal conditions.
- Cold treatment: hardened material cooled to −200°C is held in cooling units, which improves the stability and performance of cutting and measuring tools.
Thermochemical treatment of metals
Thermochemical treatment is used when the composition of a specific layer of the metal needs to be changed. The main types of this treatment include:
- Carburizing: saturating the surface with carbon, producing a part with a soft core and a hard surface.
- Nitriding: saturating the surface with nitrogen, which increases corrosion resistance and fatigue strength.
- Boriding: saturating the surface layer with boron, which increases wear resistance and resistance to acidic and alkaline environments.
- Aluminizing: saturating the surface with aluminum, which makes parts resistant to aggressive gaseous environments.
- Chromizing: saturating the surface with chromium, which increases hardness and resistance to scaling, corrosion and wear.
The thermochemical treatment process
Thermochemical treatment of metals and alloys involves heating and holding workpieces in active media containing chemical elements. This method introduces specific chemical elements into the required layers of the workpiece, changing the chemical composition and structure of the surface layers.
After treatment, a diffusion layer is formed in which not only the chemical composition but also the structure and characteristics of the surface layers have changed. Different saturating components produce different changes in the diffusion layer.
Thermochemical treatment can be:
- Single-component: saturation with one element (for example, carbon, nitrogen or chromium).
- Multi-component: saturation with several elements (for example, carbonitriding — nitrogen and carbon; boroaluminizing — boron and aluminum).
Traditional saturation methods
Industry most often uses traditional thermochemical treatment methods such as nitriding, carburizing and cyaniding. These methods reliably improve the properties of metals required for a wide range of industrial applications.
Thermochemical treatment is a complex process that requires precise control and an understanding of metal properties. This method significantly improves the performance of metal products, making them more resistant to wear, corrosion and other negative effects, which increases their durability and reliability.