How to choose the right heat treatment for different alloys

Heat treatment of metals and alloys plays a key role in improving their mechanical, physical and chemical properties. It makes it possible to achieve specific characteristics such as hardness, strength, ductility and corrosion resistance, which makes materials suitable for a wide range of industries. However, each alloy requires an individual approach to heat treatment. Let us look at how to choose the right heat treatment for different alloys, using the most common types as examples.

1. Heat treatment of steel

Steel is one of the most widely used materials in mechanical engineering and construction. There are many types of steel that differ in chemical composition and therefore require different heat treatment conditions.

  • Carbon steel. For low-carbon steel (up to 0.25% carbon), normalizing and annealing are the optimal processes. Normalizing refines the grain structure of the metal, increasing its strength and ductility. Medium- and high-carbon steels are most often hardened and then tempered: hardening makes the steel hard, and tempering reduces its brittleness.
  • Alloy steels. Depending on the alloying additions (chromium, nickel, molybdenum), alloy steels may require more complex treatment cycles. For example, chromium steels are hardened from 850–900 °C and then tempered to relieve stresses.

The right choice of treatment for steel depends on the requirements for the finished product. If high strength and wear resistance are needed, hardening and tempering are used. If ductility and weldability are important, normalizing and annealing are preferred.

2. Aluminium alloys: choosing temperatures and treatment conditions

Aluminium alloys are distinguished by high corrosion resistance and low weight, which makes them indispensable in the aviation, automotive and construction industries. However, their heat treatment requires precise temperature control to avoid loss of properties.

  • Solution treatment. The main heat treatment for aluminium alloys is solution treatment followed by ageing. Solution treatment is usually carried out at 450–550 °C, followed by rapid cooling, as a rule in water. This produces a supersaturated solid solution, which provides strengthening during subsequent ageing.
  • Ageing. After solution treatment, the alloys undergo natural or artificial ageing. Natural ageing takes place at room temperature over several days, while artificial ageing requires heating to 150–200 °C, which speeds up the process.

The choice of a specific heat treatment for aluminium alloys depends on their grade. For high-strength alloys (such as duralumin), solution treatment followed by artificial ageing is preferred to achieve maximum strength.

3. Magnesium alloys: temperature conditions and their effect on properties

Magnesium alloys are used in aircraft and automotive manufacturing thanks to their low weight and high specific strength. However, their heat treatment requires a special approach because magnesium is sensitive to high temperatures and prone to structural changes.

  • Annealing. To improve ductility, magnesium alloys are annealed at 300–400 °C. This process relieves internal stresses that arise during casting or cold working.
  • Solution treatment and ageing. Like aluminium alloys, magnesium alloys are strengthened by solution treatment followed by ageing. Depending on the grade, solution treatment is carried out at about 380–530 °C and artificial ageing at 150–250 °C. Because magnesium oxidises readily and can ignite, heating is carried out in a protective atmosphere. This improves mechanical properties such as hardness and strength.

The right choice of temperature and treatment time for magnesium alloys depends on the required final properties of the material, such as strength or ductility.

4. Titanium alloys: complex treatment for maximum strength

Titanium is used in the aerospace and medical industries thanks to its unique combination of low weight, strength and corrosion resistance. However, its heat treatment requires careful selection of conditions, because at high temperatures titanium actively absorbs oxygen and forms a brittle oxidised surface layer.

  • Annealing. The main heat treatment for titanium is annealing, carried out at 700–900 °C. Annealing reduces internal stresses, improves ductility and increases impact toughness.
  • Solution treatment and ageing. Titanium alloys such as Ti-6Al-4V undergo solution treatment at 900–950 °C followed by ageing at 480–600 °C. This achieves high strength while maintaining corrosion resistance.

The right heat treatment for titanium depends on the requirements for the finished product and its performance characteristics. Precise temperature control is important to prevent embrittlement and loss of corrosion resistance.

5. Copper alloys and bronzes: choosing gentle treatment

Copper and bronze are used in electronics and construction thanks to their high conductivity and corrosion resistance. Their heat treatment is aimed at improving ductility and reducing internal stresses.

  • Annealing. Copper alloys are annealed under gentle conditions at 400–600 °C, which improves workability and relieves internal stresses.
  • Quenching. Unlike steel and aluminium alloys, most copper alloys are rarely quenched, as this does not significantly increase their hardness. The exceptions are precipitation-hardening alloys such as beryllium bronze. The main focus is on annealing and slow cooling.

Choosing the right heat treatment for different alloys requires taking into account their chemical composition, the required mechanical properties and the field of application. Control of temperature, holding time and cooling plays a key role in achieving the optimal properties of the material.

°C
Need heat treatment of metals?
We perform heat treatment of metal parts: hardening, tempering, normalizing and other processes. Learn about our capabilities, technical parameters and order terms.
Learn more about the service →
Scroll to Top