Heat treatment (hardening) of metal in salt baths

Hardening is an important stage of metal heat treatment that significantly improves the mechanical properties of parts. One effective way to carry out hardening is to use protective media, such as a quenching salt bath and special process coatings. These methods help minimize or completely eliminate oxidation and decarburization, ensuring a high-quality surface on the treated parts.

Hardening in a salt bath

We offer treatment of parts in the protective medium of a quenching salt bath. During this treatment, the parts are heated to the hardening temperature in a specially formulated salt composition. This method has several key advantages:

  • Minimal oxidation: Oxidation processes are virtually absent in a salt bath, which greatly reduces the risk of scale forming on the surface of parts.
  • Protective film: When parts are removed from the molten salt, a thin protective film forms on their surface and shields them from atmospheric oxygen. During quenching, this film comes off on its own without leaving any marks on the parts.
  • High surface quality: Parts hardened in a salt bath retain a smooth, clean surface, which reduces the need for further finishing.

This hardening method is especially effective for parts that require high precision and surface cleanliness, such as precision mechanism components and tools.

Hardening with protective coatings

Another common hardening method is the use of protective process coatings. This method also aims to prevent oxidation and decarburization of parts during high-temperature heating. The advantages of hardening with protective coatings include:

  • Protection against oxidation and decarburization: Protective coatings shield parts from oxygen and carbon exposure, preserving the original properties of the material.
  • Self-removing coating: During cooling, the coating flakes off the parts on its own due to differences in linear expansion coefficients. This eliminates the need for additional cleaning.
  • Lower machining effort: Protective coatings reduce the consumption of expensive cutting tools and the amount of machining required, which lowers the cost of manufacturing parts.

The coating process consists of several stages:

  1. Cleaning the parts: Parts are first cleaned of dirt and oil to ensure better adhesion of the coating to the surface.
  2. Heating the parts: Parts are preheated to improve coating adhesion.
  3. Applying the coating: The coating is applied by dipping or spraying in two coats, with intermediate drying for 10–20 minutes.

This method is suitable for a wide range of parts, including those used in aggressive environments and requiring high performance.

Benefits of using protective media

Using protective media during hardening provides the following benefits:

  • Better surface quality: Parts protected from oxidation and decarburization have a higher-quality surface, which simplifies subsequent machining.
  • Lower production costs: Reduced machining effort and cutting tool consumption lower overall production costs.
  • Longer service life: Protective media help extend the service life of parts by improving their mechanical properties and corrosion resistance.

Hardening in protective media, such as salt baths and process coatings, is an effective method of metal heat treatment. These technologies significantly improve the surface quality of parts, reduce production costs and extend product service life. Our company offers high-quality hardening services in protective media, delivering reliable and durable results for various types of parts. Contact us for a detailed consultation and to place an order for heat treatment.