For several years, our company has been cooperating with many valve manufacturers in Ukraine, for which we perform nitrocarburizing of the main and auxiliary parts of shut-off valve assemblies.
Thanks to our treatment, the service life of the mechanisms has increased several times, which has made it possible to reduce the costs of manufacturing new assemblies.